| Parameters | |
|---|---|
| Factory Lead Time | 3 Weeks |
| Material | Polyolefin (PO), Irradiated |
| Operating Temperature | -55°C~135°C |
| Packaging | Spool |
| Published | 2002 |
| Series | SH275 |
| Feature | Abrasion Resistant, Flame Retardant |
| Part Status | Active |
| Moisture Sensitivity Level (MSL) | Not Applicable |
| Type | Tubing, Flexible |
| Max Operating Temperature | 135°C |
| Min Operating Temperature | -55°C |
| Color | Black |
| Shrinkage Ratio | 2 to 1 |
| Shrink Temperature | 90°C |
| Diameter | 25.4mm |
| Length | 100.0' 30.5m |
| Diameter - Inner, Supplied | 1.000 (25.40mm) |
| Diameter - Inner, Recovered | 0.500 (12.70mm) |
| Recovered Wall Thickness | 0.035 0.89mm |
| RoHS Status | ROHS3 Compliant |
| Lead Free | Lead Free |